5000 high early strength concrete mix has a walk on time of 10 hours to 12 hours.
Quikrete high strength concrete mix instructions.
This concrete mix is designed for applications requiring high early strength and rapid strength gains.
When working with cement based products always wear eye protection and waterproof gloves.
Table 1 typical compressive strength1 compressive strength astm c39 age typical values 7 days 2500 psi 17 2 mpa 28 days 4000 psi 27 6 mpa slump range 2 3 51 76 mm.
Quikrete concrete mix exceeds the compressive strength requirements of astm c387 as shown in table 1.
The use of this quality mixture ensuring your finished project will last you for years to come.
Q 5000 concrete mix consists of a commercial grade blend of portland cement sand gravel.
Then add 3 quarts of water for every 80 pounds of quikrete and use a hoe to mix the water and concrete together.
Sidewalks driveways setting posts.
Sakrete high strength concrete mix is a preblended mixture of sand coarse aggregate and cementitious materials.
For new construction or repairs where concrete thickness exceeds 2 inches you ll want to count on a preblended mixture that can.
Properly graded sand and gravel blended with portland cement for use as in general concrete applications.
Next put the desired amount of quikrete mix into a wheelbarrow or mortar tub and make a hole in the middle.